Composite or steel rebar?
A comparison without the marketing: where composite brings savings and durability, and where the structural calculation decides — with figures from the tests on our rebar.
1,000+ MPa
average tensile strength of our rebar, tested in 2023
≈ 5 ×
lighter than steel rebar of the same diameter
100 m
in a single coil — no splices every 6 m
Comparison
Property by property
Composite isn't “better steel” — it's a different material. It is stronger in tension and doesn't rust, but it is less stiff. That determines where it should be used.
| Property | Composite (fibreglass) | Steel (B500) |
|---|---|---|
| Corrosion | does not corrode — moisture, salt and chemicals don't attack it | corrodes; rust expands and breaks up the concrete around the bar |
| Tensile strength | 1,036.5 MPa (Ø8) and 1,022.0 MPa (Ø10) our rebar, reports 136 and 137/2023 | yield strength 500 MPa |
| Modulus of elasticity | at least 50 GPa for type ASK, to GOST 31938-2022 | 200 GPa — about four times stiffer |
| Weight, Ø8 | 0.080 kg/m measured | 0.395 kg/m |
| Weight, Ø10 | 0.134 kg/m measured | 0.617 kg/m |
| Up to failure | elastic — no yielding | yields and deforms visibly before failure |
| Electricity and magnetism | non-conductive; doesn't interfere with radio waves or sensitive equipment | conductive; magnetic |
| Temperature | the resin softens above the glass transition temperature — at least 90 °C under GOST 31938-2022 | keeps its load-bearing capacity up to much higher temperatures |
| Supply | 50 and 100 m coils or bars from 1 to 8 m and cut to length | bars from 6 to 12 m, a lorry and a crane |
| On site | cut with bolt cutters or an angle grinder, tied with wire; cannot be permanently bent | cut with an angle grinder; can be bent and welded |
Where it pays off
Wherever steel rusts.
Composite's biggest advantage isn't the price per metre, but the fact that the concrete around it doesn't deteriorate. Where steel is constantly exposed to moisture and salt, that means a building without repairs.
In Montenegro this is no exception: much of the building happens by the sea, and paths, driveways and car parks in the north are salted in winter.
-
Seafront buildings
Salt in the air and water destroys steel reinforcement even when the concrete is good. Composite doesn't corrode.
-
Car parks, driveways and ramps
De-icing salts and water from vehicles get into the concrete — that is exactly where steel deteriorates fastest.
-
Ground-bearing floors, paths and paved areas
Here the reinforcement mainly prevents cracking, and the concrete is in constant contact with moisture from the ground.
-
Tanks and water structures
Constant moisture with no way of repairing the reinforcement — a typical place for composite.
-
Substations, laboratories, MRI rooms
Composite doesn't conduct electricity and isn't magnetic, so it doesn't interfere with measuring and medical equipment.
-
Facades and cladding
No rust means no stains on the stone or facade, and no cracking of the cladding from corrosion.
Where it needs calculation
Where composite isn't a simple replacement
These aren't reasons against composite, but places where the structural engineer decides on it — often in combination with steel in the same structure.
Longer-span beams and slabs
A lower modulus of elasticity means greater deflection under the same load — here deflection, not load-bearing capacity, often determines the dimensions.
Load-bearing building elements
Composite is elastic up to failure, without yielding like steel — so the codes require a larger load-bearing reserve.
Fire and heat requirements
The resin softens at elevated temperatures, so the concrete cover and the use are determined by calculation.
Bent elements
Stirrups and hooks aren't bent on site — they are provided for in the design in advance, or steel is used there.
Design standards and guides (GOST, SP, ACI 440.1R) and the test reports are on the technical documentation page.
Savings
Where the savings really show
The price per metre depends on the diameter and quantity, so we calculate the savings for each specific project. But some items always count in composite's favour.
- Transport: 1,000 m of Ø8 rebar weighs 80 kg in composite and 395 kg in steel.
- Unloading and handling: coils are carried by hand — no crane or forklift.
- Waste and splices: a 100 m coil has no laps every 6 m.
- Tools: cut with bolt cutters, no power or cutting discs needed.
- Maintenance: no corrosion repairs over the life of the building.
Worldwide experience
Nothing new — just new here
GFRP rebar has been designed and installed for decades — in bridges, metro systems, car parks and laboratories around the world.
-
1978
The USSR publishes recommendations for the design of structures with fibreglass reinforcement (R-16-78, NIIZhB).
-
1986
In Germany, composite is installed in a road bridge — the start of its use in Europe.
-
1997
Japan, with more than a hundred commercial projects by the mid-1990s, gets design recommendations. In Canada, the Headingley (Manitoba) and Joffre (Quebec) bridges open.
-
2006
The covered car park of the Forum Steglitz shopping centre in Berlin — a mesh of Ø8 bars over 6,400 m², against corrosion and cracking.
-
2018
The Faculty of Civil Engineering in Podgorica publishes research on continuous beams with GFRP reinforcement.
-
today
Used in the metro systems of Berlin, London, Bangkok, New Delhi and Hong Kong, in MRI rooms and in laboratories sensitive to electromagnetic interference.
Frequently asked questions
What we're asked most often
Can composite fully replace steel rebar?
In ground-bearing floors, paths, paved areas, retaining walls and facades — usually yes. In beams, longer-span slabs and load-bearing building elements the structural engineer decides, and composite is often combined with steel in the same structure.
Is composite rebar brittle?
It doesn't break easily — our rebar withstands over 1,000 MPa in tension, twice the yield strength of B500 steel. But it doesn't yield like steel: it behaves elastically up to failure, so a larger reserve is used in the calculation.
How long does it last?
Composite doesn't corrode, so there is none of the process that shortens the life of concrete with steel by the sea and in damp conditions. Resistance to aggressive media is tested under a separate standard, GOST 32487-2015.
What composite diameter replaces a steel one?
It depends on the element and the design — because of the lower stiffness there is no single replacement table for every case. For mesh there is an indicative replacement, listed in the mesh catalogue; for load-bearing elements the diameter is specified by the structural engineer.
Does composite pay off on your project?
Send us the rebar specification from the design or a description of the building — we'll reply with a price for the composite option and a delivery time.